V2A is a stainless steel grade. In fact for marine applications Monel metal ( a high nickel alloy) is preferred, since stainless steels suffer from a phenomenon called chloride cracking.

Steve

List of 20 messages in thread
TopicAuthorDate
Deep sea application            01/01/70 00:00      
   RE: Deep sea application            01/01/70 00:00      
      RE: Deep sea application            01/01/70 00:00      
   RE: Deep sea application            01/01/70 00:00      
      RE: Deep sea application            01/01/70 00:00      
         RE: Deep sea application            01/01/70 00:00      
            RE: Deep sea application            01/01/70 00:00      
               RE: Deep sea application            01/01/70 00:00      
                  RE: Deep sea application            01/01/70 00:00      
                     RE: Deep sea application            01/01/70 00:00      
                        RE: Deep sea application            01/01/70 00:00      
   RE: Deep sea application            01/01/70 00:00      
      Spoken like a true engineer!            01/01/70 00:00      
         RE: Spoken like a true engineer!            01/01/70 00:00      
            RE: Spoken like a true engineer!            01/01/70 00:00      
      RE: Deep sea application            01/01/70 00:00      
         RE: Deep sea application            01/01/70 00:00      
         RE: Deep sea application            01/01/70 00:00      
      RE: Deep sea application            01/01/70 00:00      
      RE: Deep sea application            01/01/70 00:00      

Back to Subject List